I'm looking for small (a lb) quantities of frits that would
separate the effects of calcia, magnesia and phosphorus on iron
glazes, and am having problems finding sources.

First, I need a frit free of all of these that will allow a clean
silica+alumina+iron oxide mix to fully melt at cone 6. Fusion
makes several that look as though they should work: F-15, 74, 367
and 492.

Then, I need an insoluble source of calcia+phosphorus-free Mg
such as Fusion F-69.

Finally, I need an insoluble Ca+Mg-free source of P2O5, and
haven't located anything.

Emails to Fusion, Ferro and Pemco have gone unanswered. Does
anyone know of a possible source of any such frits?

--