Kiln wash that works for one kind of shelf may not work for another. Our
Salt kiln wash for Silicon Carbide shelves loves to flake from our Thorley
Shelves.
Louis
I will be at the NCECA Symposium next week and off line much of the time.

Talbott on mon 10 nov 97

The Lee's Kiln wash from Axner will not flake off... I use it on my nitride
bonded silicon carbide shelves from New Castle Refractories and I have had
terrific results. .. Marshall

>----------------------------Original message----------------------------
>Kiln wash that works for one kind of shelf may not work for another. Our
>Salt kiln wash for Silicon Carbide shelves loves to flake from our Thorley
>Shelves.
>Louis
>I will be at the NCECA Symposium next week and off line much of the time.

101 CLAYART MUGS... A TRAVELING EXHIBIT
2ND ANNUAL CLAYARTERS' GALLERY - NAPLES, MAINE (Summer 1998)
E-MAIL ME FOR AN APPLICATION
http://fmc.utm.edu/~dmcbeth/cag/naples.htm

Celia & Marshall Talbott, Pottery By Celia, Route 114, P O Box 4116,
Naples, Maine 04055-4116,(207)693-6100 voice and fax,(call first)
Clayarters' Live Chat Room, Fri & Sat Nites at 10 PM EDT & Sun at 1 PM EDT
http://webchat12.wbs.net/webchat3.so?Room=PRIVATE_Clayarters
---------------------------------------------------------------------