I was wondering if someone could suggest Frit substitutions for Frit 111,
Frit 146 and 156. These were suggested for the copper red article in '97
November CM pages 106-107.
Thanks
Ron Roy on tue 11 nov 97
>----------------------------Original message----------------------------
>I was wondering if someone could suggest Frit substitutions for Frit 111,
>Frit 146 and 156. These were suggested for the copper red article in '97
>November CM pages 106-107.
>
>Thanks
Who makes those frits - if we have analysis for them it's a piece of cake.