tom coleman porcelain body

updated thu 13 nov 97

 

Donald G. Goldsobel on mon 10 nov 97

Last April I received samples of tom Coleman's porcelain body at Nceca. I
finally go around to trying and found it throws better than my regular
body, Dave's Porcelain from Laguna.

Does this body fire pure white in reduction? Who distributes it in the
Southern California area? Any comments on your experience with it at cone
10 in reduction will be appreciated.

Thanks a heap
Donald Goldsobel in the sunny San Fernando Valley where winter hasn't
showed any sign of coming around.

Jean Stephenson on wed 12 nov 97

You can buy Coleman Porcelain from Aardvark in Santa Ana. It's
wonderful stuff, isn't it? If you are in the Southern Oregon or N.
Calif. area you can also get the porcelain from Southern Oregon Pottery
and Supply in Talent, OR. Good luck. Jean