Randy McCall on sun 23 dec 07


I have been experimenting with layering Chappell's Floating Blue base.
Check out the casserole on my main web page. You may have to scroll down to
see it.

I call it Green Moonrock.

Layered Chappell's Floating Blue using cobalt carb on the bottom, and same
base but used rutile 4% and copper carb 4% on top. Sponged on top glaze one
layer. Fired to a hard cone 6 no slow firing up or down. Got great
movement and variation.


Randy