search  current discussion  categories  glazes - misc 

rescue glaze test results

updated sat 29 dec 07

 

Ingeborg Foco on fri 28 dec 07


I think that was the name of the glaze. Someone was asking for test results
and I threw some samples in my last firing to ^10....well it only actually
went to ^9 Reduction.

The glaze came out a smooth buttery violet and when applied very heavy did
not run off the vertical sample. I brushed the glaze onto a sushi plate
glazed in a color that isn't too popular and quite frankly it added a nice
change, came out different and better. Time will tell if that will sell
but it is an improvement for sure. I did not do any acid tests yet so can't
comment on the durability of this glaze.

Hope that helps whoever was interested in this glaze.
--
Sincerely,

Ingeborg

www.thepottersworkshop.com