search  current discussion  categories  kilns & firing - cones & controllers 

electric kiln help - now kiln controllers

updated fri 18 jan 08

 

William & Susan Schran User on thu 17 jan 08


On 1/16/08 8:17 AM, "newt and amy" wrote:

> any suggestions on how to retrofit ? not certain if i should try to get a
> computer driven controller or should i try to add a cone setter. i only
> use the electric kiln for bisq.

You can buy wall mounted kiln controllers.
Here's some examples:

http://www.skutt.com/products/kmcntrl.html

http://www.amaco.com/prod-select-fire-wall-mount-145.html

http://www.evenheat-kiln.com/accessories/rm2hh/rm2hh.htm


Bill


--
William "Bill" Schran
wschran@cox.net
wschran@nvcc.edu
http://www.creativecreekartisans.com