Maggie Jones on sun 20 jan 08
I always get confused...Jigger is: similar to hump molds..and Jolley is:
...slump mold?
thanks
maggie
http://TurtleIslandPottery.com
Maggie and Freeman Jones
On Sun, 20 Jan 2008 13:00:21 -0700 James and Sherron Bowen
writes:
> Jolleying -(NOTE SPELLING) Shaping of hollow ware by means of a
> profiled at
> a fixed distance from the rotating surface of a hollow plaster
> mould.
> JB
> ----- Original Message -----
> From: "Jonathan Kaplan"
> To:
> Sent: Sunday, January 20, 2008 10:23 AM
> Subject: Jigger/Jolly
>
>