Jonathan Kaplan on sun 20 jan 08
I have read the recent threads on jiggering and jollying that have
been posted recently.
Having used this process for more years than I wish to date myself,
if anyone wants to post me off the list with particular questions, I
would be happy to address them.
Respectfully,
Jonathan
Jonathan Kaplan
Ceramic Artist/Ceramic Designer
Master Mold and Model-Maker
Plinth Gallery/Ceramic Design
3520 Brighton Blvd
Denver, CO 80216
www.plinthgallery.com
303 909-5488 cell
303 295-0717 office
James and Sherron Bowen on sun 20 jan 08
Jolleying -(NOTE SPELLING) Shaping of hollow ware by means of a profiled at
a fixed distance from the rotating surface of a hollow plaster mould.
JB
----- Original Message -----
From: "Jonathan Kaplan"
To:
Sent: Sunday, January 20, 2008 10:23 AM
Subject: Jigger/Jolly
| |
|