search  current discussion  categories  glazes - cone 4-7 

^6

updated sat 26 jan 08

 

Collette Smith on tue 22 jan 08


Has anyone out there done ^6 Reduction firing and have formulas?
C.Smith

primalmommy on fri 25 jan 08


Yes, there are potters working in ^6 reduction.

Diana Pancioli has done a lot of work with ^6 reduction glazes. That's
all we fire in the gas kiln at EMU.

You can check out her results at glazeforward.com and if you are
interested, she'll send you the "recipes" and a box of actual glaze
samples, to look over, and then forward to the next person on the list.

Hth!

Yours
Kelly Savino in Ohio

http://www.primalpotter.com
http://www.primalmommy.com/blog.html