Roxanne Hunnicutt on tue 5 feb 08


>
> Dear Kendra and all:
>

Here is a Leach Clear with a satin finish that does r/ox ok

Calling it Leach is not really correct as it has been revised to Cone six!

custer 25
whiting 25
silica 25
kaolin 25
frit 3124 15

I KNOW: Total is not 100. Maybe someone want to work on that? But I like
using these numbers as they are mostly consistant! Rox in OR

>
> Date: Mon, 4 Feb 2008 11:47:25 -0600
> From: Digital Studio
> Subject: Clear Glaze
>
Kendra Bogert
www.digital-studio.biz

> I'm looking for a clear cone 6 glaze. This seems simple enough but I
> want one that keeps the original color of our bisque (nice toasty manila
> color). I have mixed this variation of Waterfall Brown and it looks
> amazing:
> Base Glaze of Waterfall Brown, plus
> Rutile 1
> 3195 Frit +3% (29% total)
>
> You can see this one on my Flickr:
> (http://www.flickr.com/photos/digitalstudio) It's the one called
> Waterfall White. I'm wondering how I can get that clear color that keeps
> the color of the bisque in this glaze /without/ the white waterfall
> part. Would the base of Waterfall work for this?
>
>
> --
> Kendra Bogert
> www.digital-studio.biz
> 641-208-6253I WISH YOU all of the best of life: Free and light-hearted
> laughter, all the riches of the heart, such as a loving and supportive group
> of family and friends, a true and constant belief in your own worth and
> abilities, intellectual curiosity and a serene state of mind.
>