Hi

I bought the chinese 3/8" carbide shelves from geil and they have
cracked or broken and he hasn't replaced any and its been two years now.

Bryan Hannis

Bryan Hannis on sat 1 mar 08


Hi

Mice or men?? My shelves were well packed and delivered on time, but
2 had small cracks, when fired once the cracks spread, Geil was
notified. Quote " we are having trouble with these shelves, but will
replace them for you". Great I said. Quote " could you take some
pictures and email them to me", I did, after numerous emails and
calls I gave up and moved on. I would never buy anything from him or
his company ever again.

Bryan Hannis