search  current discussion  categories  tools & equipment - pug mills 

pug mills.. venco

updated wed 19 nov 97

 

Talbott on tue 18 nov 97

With our Venco 4" deairing pugmill we typically get 90 kPa of vacuum or
better. You should easily be able to pug and deair 1000 lbs of clay per
hour even with a 4" Venco. However, they do make larger models. Axner can
give you a lot more details..

Note: (101 kPa is equivalent to 1 atmosphere or 760 mm Hg or 14.7 psi)

.....Marshall

101 CLAYART MUGS... A TRAVELING EXHIBIT
2ND ANNUAL CLAYARTERS' GALLERY - NAPLES, MAINE (Summer 1998)
E-MAIL ME FOR AN APPLICATION
http://fmc.utm.edu/~dmcbeth/cag/naples.htm

Celia & Marshall Talbott, Pottery By Celia, Route 114, P O Box 4116,
Naples, Maine 04055-4116,(207)693-6100 voice and fax,(call first)
Clayarters' Live Chat Room, Fri & Sat Nites at 10 PM EDT & Sun at 1 PM EDT
http://webchat12.wbs.net/webchat3.so?Room=PRIVATE_Clayarters
---------------------------------------------------------------------