search  current discussion  categories  materials - frits 

frit 3195: id on #50 bag?

updated mon 7 apr 08

 

Eleanora Eden on sun 6 apr 08


I just opened a 50 lb bag of Ferro Frit 3195 that I bought from my supplier.
I am surprised to find no ID at all on the bag that says it is 3195.
In large print
at the top of the front of the bag it says "#16AM".

The only other # I can find on the bag is (CAS #65997-18-4) which seems to be
some NIOSH labelling about chemical exposure.

I can't use this stuff until I know it is what I bought. I looked it
up on Ferro and
don't find any information. I sent them a query and hope to get a response.

Anybody have a clue about this?

Thanks,

Eleanora
--
Bellows Falls Vermont
www.eleanoraeden.com