amblygonite was spodumene

updated sun 20 apr 08

 

Lee on sat 19 apr 08


See Amblygonite gem here:

http://www.mindat.org/photo-1226.html


Amblygonite: (Li,Na)AlPO4(F,OH)
Spodumene : LiAl(SiO3)2




--
Lee, a Mashiko potter in Minneapolis