search  current discussion  categories  glazes - misc 

4x4 recipe/again

updated sat 26 apr 08

 

mel jacobson on fri 25 apr 08


mark, i posted it last week, and about four other times
on clayart.

equal parts:
china clay
feldspar
silica
ball clay.

use what you have.
as you know, if you turn this around, increase
the feldspar and silica you have the perfect clear
glaze for this clay body.
mel