search  current discussion  categories  glazes - specific colors 

green glaze correction

updated fri 21 nov 97

 

Rich Germer on thu 20 nov 97

I sen t a message yesterday regarding a matte green glaze that drips to a
sort of metallic gray and fires to cone 9 oxidation. I gave my email address
for any responses but it was wrong! My email address is rgermer@semmcoop.com

My previous message read as follows:
Does anyone know of a recipe for a green glaze--a somewhat bright green,kelly
green or similar--that is matte, drips to a sort of metallic gray, and fires
to cone 9 OXIDATION? I saw someone who had this glaze but he would not reveal
the recipe. If anyone has any clues or helpful hints I would appreciate it.

My CORRECTA email address is rgermer@semcoop.com
email address is rgermer@semcoop.com

Rich Germer