Deborah Thuman on wed 28 may 08
I've never had luck getting clay off anything I've used as any kind of
mold unless I first put something between the mold and the clay. My
somethings that work best are: wet paper towel or plastic wrap.
Deb Thuman
http://debthumansblog.blogspot.com/
Jeanette Harris on wed 28 may 08
>I've never had luck getting clay off anything I've used as any kind
>of mold unless I first put something between the mold and the clay.
>My somethings that work best are: wet paper towel or plastic wrap.
Old panty hose.
--
http://jeanetteharrisblog.blogspot.com/
http://www.washingtonpotters.org/members/Jeanette_Harris/wpa_jeanette_harris.htm
http://www.sa-clayartists.org Click on Members, then H
Jeanette Harris
Washingzona
| |
|