Dear Group;

I use the Stainless Steel soft-annealed wire from this supplier. .009 =20=

or .010 is great for fine wires, .012 for meduim ones, and .014 for =20
coarser wires. I use this wire in Hank's CutOff Wires as well as =20
Hank's WireTool. It is great twisted together to make wires for =20
cutoff and faceting. I have never tried the stranded wire. Order =20
pages at bottom of message.

Cheers! Hank in Eugene

Begin forwarded message:

> From: "Mark Fazzio"
> Date: May 30, 2008 3:49:21 PM PDT
> To: "Hank Murrow"
> Subject: RE: Highland Metals
>
>
> The 1 lb spools are listed on page 4 under
>
> Wire Ligatures
>
> Ligature Wire, 1 lb spool @ $19 per spool, or 6 spools for $18 each.

> They are available in sizes .009, .010, .012 and .014 (see note =20
> above).
>
> We do carry Stranded Stainless Steel wire in spools - these are listed
> on page 3 under Stranded SS. They are available in sizes .0155, .0175
> and .0195 in 3 Strand Spools or 7 Strand spools.
>