search  current discussion  categories  materials - clay 

derniere cuisson; lime pops

updated tue 3 jun 08

 

Lili Krakowski on mon 2 jun 08


M le docteur Bastarache!!!!!!!!!! I misread! As long as it is only derniere
cuisson, and NOT derniere cuisse, it is ok! Salut.

Larry. I knew it was Neph Sy because that is what was in there! I forget
what the body was. It was old NephSy clumped, we thought, from dampness,
and just did not dissolve as it should have had it been bone dry. ("We"
means Hobart Cowles and me--I showed the defective pots to him)

I must look up Cardew on the order of putting plastics and non plastic
materials in the slurry. But anyway I ever since have sieved non plastics
and some clay into a slurry together.



Lili Krakowski

Be of good courage