Hi Clayart

John Britt was kind enough to send me some recipes for Oil Spot glazes at
cone 6.
All of the tests you can see at my flickr site, Oil Spot album.

http://www.flickr.com/photos/glazes/sets/

I think there were some interesting results, especially the combo glazes
with colorants. There were also some tea dust effects, if not spots. I will
want to make some further experiments with these glazes, also the cover
glaze #2 over other iron rich glazes I regularly use in my studio.

Thanks John.