search  current discussion  categories  glazes - crazing & crackle 

raku clear crackle glaze

updated tue 25 nov 97

 

John H. Rodgers on sun 23 nov 97

-- [ From: John H. Rodgers * EMC.Ver #2.5.02 ] --

I need for raku a clear crackle glaze that can stand alone as well as serve
as a good crackle base glaze for stains or other colorants.

Anyone?

TIA

John Rodgers
Enjoying a beautiful day in Alabama

Michelle H. Lowe on mon 24 nov 97

Here's a real nice one I've been using that fits all these requirements

Large Crackle

Gerstley 60
Spodumene 35
Kentucky Ball Clay 5

TOTAL 100


At 07:39 PM 11/23/97 EST, you wrote:
>----------------------------Original message----------------------------
>-- [ From: John H. Rodgers * EMC.Ver #2.5.02 ] --
>
>I need for raku a clear crackle glaze that can stand alone as well as serve
>as a good crackle base glaze for stains or other colorants.
>
>Anyone?
>
>TIA
>
>John Rodgers
>Enjoying a beautiful day in Alabama
>
>
Michelle Lowe, potter in the Phoenix desert \|/ |
mishlowe@indirect.com -O- | |
mishlowe@aztec.asu.edu /|\ | | |
|_|_|
http://www.amug.org/~mishlowe ____ |
-\ /-----|-----
( )
<__>