kdholman on sun 23 nov 97
I have a 15 gallon pressure pot and I was wondering if anyone know's
what would be the Specific Gravity or Centipoise I should keep my Glaze
at.Is there a harm in using Darvan to thin out the glaze? and is Epson
salt ok to use,or would it be better to use V-gum Ceramics.I use a Frit
base glaze and fire to cone 4 2080/F and soak for 45min.Looks like some
of the pots have Crawling ?
| |
|