Bonnie Hellman on sun 15 jun 08
Hi clayarters,
Linda Blossom asked me to post this additional message. She has one more =
thing to add to her email about ceramic items for sale. Please contact =
her with questions, etc.
Bonnie
I forgot to add that the super kiln has a type s thermo couple. I also =
have a 12" Type S with a pyrometer for my gas kiln but which could be =
used with electric. Type S unlike the others, is very accurate and will =
outlive the owner. the 12" one has never been used and I believe I paid =
$300 for it about a year ago or less. If you are interested, please =
email me at:
lindajblossom at gmail.com
Linda
Below is a re-posting of her original email.
I am finally ready to sell my studio equipment. I am still in DC and =
working for a union in their research library. I don't think my clay =
days are behind me but architectural work is and I simply won't have a =
place for the equipment and supplies. Here is a list of what I have =
and where it is. I don't have all the prices figured out yet, but if =
there is something you are interested in, please email me. I know there =
is more there than I have listed here and hopefully when I know better =
what is happening, I can come to NY and deal with it personally. =
Meanwhile, this is a heads up on part of what I will be selling. =20
In the DC area, these things are here:
Beam central vacuum
stains - at least 60 Mason stains and some Degussa. Many colors and =
most 1 lb.
sculpture stand
large turntables for making large objects - 3
a few rod tile setters from Laguna (rest in NY)
=20
In Ithaca, NY, I am in Dc typing this from memory so I can't go and =
check for names and measure things:
Axner Super Kiln - the largest one, coated with ITC, more than enough =
shelves and posts. Fired less than 100 times.
12 x 24 shelves for the gas kiln - I don't have a count but there are =
quite a few.
a few wider and a few narrower shelves as well, probably 8" and 15"
Bailey 40" electric slab roller - the original with the large rollers =
which does well with thick slabs.
Georgini tile press
Bailey pneumatic extruder with cut off shelf, wall stand, and expansion =
box, 4" barrel, dies for both barrels.
Lots of 2x 4 shelving that uses shelf links for assembly
Spray booth - I don't remember the brand (something with the word creek =
in it)- it came from Axner, has a squirrel cage motor and was $500 new. =
It is close to 4' wide.
10" MK tile saw and stand. This was at least $900 new and has light =
duty.
diamond blade bandsaw for cutting tile and glass on the curve especially =
mosaics. It was at least $500 new. Diamond Tech maybe is the brand. =20
hvlp Titan sprayer and turbine.
rod tile setterss from Laguna
7" stackable tile setters
8" stackable tile setters
shelf like tile setters - the square boxes with shelves that you =
insert. I think there are 5-6 of these. They have single, 7" shelves.
glaze and clay chemicals that I just don't know what they all are from =
here - they are in NY
Peter Pugger - non deairing pugmill - the largest one which runs about =
$5740 right now. It has had very light duty. It is the PM-100 which =
handles up to 250 lbs. People have expressed an interest in this. I =
would probably look to get $3000 for it.
EZ UP tent
forms for making pedestals
lots of small miscellaneous tools like the hacksaw with piano wire for a =
cutter.
Not clay but I will probably sell my Honda 450 Rebel. I have no place =
to put it under cover here so bringing it to DC doesn't look possible. =
I don't know that I will be here forever, but it is home for now.
I also have a relatively new invisible fence unit and at least 3 =
collars.
Linda Blossom
email: lindajblossom at gmail.com
phone: 607-280-5454
| |
|