Z Jacobson on mon 28 jul 08


Hi Anne Marie=2C
=20
I am pretty into low fire glazes and whats available. I am always looking f=
or new things to try and there are not a lot of specialty glazes out there =
in the commercial world that do what your talking about. There are a ton of=
crackle or textural crackle glazes which are pretty cool but those are dif=
ferent. What I do is buy commercial glazes when I want a matt=2C semi=2C gl=
oss or crackle color but most of the special glazes I make. The only glaze =
I have found out in the commercial world which is kind of like what your ta=
lking about is Satellite makes a textural glaze called Moon Rock which I ha=
ve layered with other colors. You can google crater glazes and find lots of=
recipes. Most will have Silicon Carbide as an ingrediant that makes the la=
va or crater. Also=2C there are some globby crawl glazes which you may like=
too.
=20
Hope this helps
Z Jacobson
Wildly Energetic Ceramics
www.zjacobsonart.com