Bob Santerre on tue 5 aug 08


I'm having a problem with my Axner Oxyprobe (appx. 8 yrs old). The
oxygen readout works just fine, but the temp readout remains at 0.00 for
the entire firing (to cone 10). I called Axner/Laguna and they had no
suggestions as to why this is happening. Their best suggestion was to
send it to them and they will check it out.

Since the oxy function is working fine it seems to me the likely source
of the problem is with the electronics of meter and not with the probe
and platinum wire.

Has anyone had such an experience with their oxyprobe? Can you offer
any suggestions as to the source of the problem and possibly how to fix it?

Thanks, Bob

Arrowsic Island Pottery