Chuck T. Wagoner on wed 6 aug 08
That is the exact one in Mr. Peeler's glaze note book, short the note from
Otto to Richard. I guess I don't have to worry about posting the high Barium
glaze. I hope that potters will take heed of the dangers of Barium
Carbonate. I'm glad to se the warning on the one you Googled!
Mr. Peeler notes that he added some Bentonite and if the glaze shivers to
add some Nyph Sy.
====================================================================
Subject: Re: Glaze Free Trade Society
Chuck
This the one?
Clayart
Wagoner, Charles on tue 24 sep 02
Otto's Swedish Mat (Waxy Yellow) Cone 10 (Barium Toxic!)
Needs a lot of reduction
Feldspar 520
Whiting 90
Zinc Oxide 80
Barium Carb 210
Ball Clay 100
Flint 30
Rutile 20
Red Iron 42
Love that Google!
I'll be careful, promise.
Des
| |
|