shellie mathews on thu 14 aug 08


in Tom Colman's book "with a little help from my friends" he gives a formula
for b-mix clay body. it is: Old Hickory #5----50#, epk---20#, PV
clay---28# and talc----2. has anyone tried this? any problems? any
suggestions? thanks, shellie mathews