Hi all,
I thought I saw a post briefly when the posts were down about someone trying the b-mix. I was curious how it is to work with? and the whiteness after it has been fired. Has any one tried it? How do you like it? I tried the wood fired porcelain and find it near impossable to work with, and I am used to working with the "super white". which was no easy feet in the begining, but I want to switch to cone 10's and am looking for a white after firing .
The Pretend Potter
Jodi