search  current discussion  categories  glazes - misc 

waterfall recipes - hungry for guacamole?

updated tue 2 sep 08

 

Jamie Yocono on fri 22 aug 08


Ilene,

The base recipe is the exact one from Ron and John's book.

The lighter blue has 5% RIO and 1% Rutile.
The green uses 12% Copper carb and 1% Rutile.

I also have what I call a Waterfall Teal and a Waterfall Avocado
(http://wooditis.blogspot.com/2007_09_01_archive.html). I don't use
them often, but they seem really nice. If anyone's interested, let me
know.

All told, I think I have eight recipes that seem to work.

Jamie in Vegas
(where yesterday, there was a helicopter buzzing my neighborhood.
Today, I read about a small plane crashing nearby, which is what the
helicopter was circling. Sad.)

___________
okay I love the first and the green Please Please share...Ilene
----- Original Message -----

sacredclay on sat 23 aug 08


> The base recipe is the exact one from Ron and John's book.
>
> The lighter blue has 5% RIO and 1% Rutile.
> The green uses 12% Copper carb and 1% Rutile.
>
> I also have what I call a Waterfall Teal and a Waterfall Avocado
> (http://wooditis.blogspot.com/2007_09_01_archive.html). I don't use
> them often, but they seem really nice. If anyone's interested, let me
> know.
>
> All told, I think I have eight recipes that seem to work.
>
> Jamie in Vegas
>
Jamie, May I inquire as to what grade of rutile you are using?
Beautiful examples! Kathryn Hughes in NC

Ilene Mahler on sat 23 aug 08


es I will love them all..Ilene
----- Original Message -----
From: "Jamie Yocono"
To:
Sent: Friday, August 22, 2008 3:54 PM
Subject: Waterfall recipes - hungry for guacamole?


> ---------------------- Information from the mail
> header -----------------------
> Sender: Clayart
> Poster: Jamie Yocono
> Subject: Waterfall recipes - hungry for guacamole?
> -------------------------------------------------------------------------------
>
> Ilene,
>
> The base recipe is the exact one from Ron and John's book.
>
> The lighter blue has 5% RIO and 1% Rutile.
> The green uses 12% Copper carb and 1% Rutile.
>
> I also have what I call a Waterfall Teal and a Waterfall Avocado
> (http://wooditis.blogspot.com/2007_09_01_archive.html). I don't use
> them often, but they seem really nice. If anyone's interested, let me
> know.
>
> All told, I think I have eight recipes that seem to work.
>
> Jamie in Vegas
> (where yesterday, there was a helicopter buzzing my neighborhood.
> Today, I read about a small plane crashing nearby, which is what the
> helicopter was circling. Sad.)
>
> ___________
> okay I love the first and the green Please Please share...Ilene
> ----- Original Message -----

Ilene Mahler on mon 1 sep 08


Please send methe waterfallteal...thanks..Ilene
----- Original Message -----
From: "Jamie Yocono"
To:
Sent: Friday, August 22, 2008 3:54 PM
Subject: Waterfall recipes - hungry for guacamole?


> ---------------------- Information from the mail
> header -----------------------
> Sender: Clayart
> Poster: Jamie Yocono
> Subject: Waterfall recipes - hungry for guacamole?
> -------------------------------------------------------------------------------
>
> Ilene,
>
> The base recipe is the exact one from Ron and John's book.
>
> The lighter blue has 5% RIO and 1% Rutile.
> The green uses 12% Copper carb and 1% Rutile.
>
> I also have what I call a Waterfall Teal and a Waterfall Avocado
> (http://wooditis.blogspot.com/2007_09_01_archive.html). I don't use
> them often, but they seem really nice. If anyone's interested, let me
> know.
>
> All told, I think I have eight recipes that seem to work.
>
> Jamie in Vegas
> (where yesterday, there was a helicopter buzzing my neighborhood.
> Today, I read about a small plane crashing nearby, which is what the
> helicopter was circling. Sad.)
>
> ___________
> okay I love the first and the green Please Please share...Ilene
> ----- Original Message -----