cc b-mix rocks!

updated fri 29 aug 08

 

j isaac on thu 28 aug 08


I just thought you might like an opinion on the cont. clays new b-mix. It is awesome. I was using cone 6 "super white" and this has the versitility of raku....^6-10 and the smooth texture of porcelain. I am producing so well I am running out of room. It is well worth the 1 1/2 hour trip to go get it. It probably wouldn't take so long if I didn't have to look at every gadget and converse so much!!!!

The Pretend Potter
Jodi