search  current discussion  categories  materials - barium 

strontium frit

updated sat 30 aug 08

 

David Martin Hershey on thu 28 aug 08


Hi Lynn,

I got some F-38 a couple of years ago from US Ceramic Supply. They were
located in a very dicey part of the LA ghetto at the time... mostly a
wholesaler, but they gave me 5 lbs. Try calling these numbers and asking
for a local or web distributor.

Fusion Ceramics Inc.
330-627-2191
330-627-5821

Texas Process Engineering Services
Co. Rd. N.E. 2050
Rt. 1 Box 475 B
Mount Vernon, TX 75457
Phone: 903-537-2787

West Coast Distribution U.S. Ceramic Supply
20417 E. Walnut Canyon Rd.
Walnut, CA 91789
Phone: 323-588-2545

Best, DMH

David Martin Hershey
DMH Studio + Design
2629 Manhattan Ave #137
Hermosa Beach CA USA
90254-2447 310.379.6890
http://www.dmhstudio.com/



Lynn Goodman Porcelain Pottery wrote:
> A day or so ago I asked for sources for strontium-bearing frits such
> as P-930, F-38 or Ferro 3292. No answer as of yet. Does anyone know
> where I can buy these frits?
>

Steve Slatin on thu 28 aug 08


Seattle Pottery Supply and Tacoma Clay Art
Center both carry 3292.

Steve Slatin --



--- On Thu, 8/28/08, Lynn Goodman Porcelain Pottery wrote:

> A day or so ago I asked for sources for strontium-bearing
> frits such
> as P-930, F-38 or Ferro 3292. No answer as of yet. Does
> anyone know
> where I can buy these frits?
>
> Thank you in advance!
> Lynn
>
>
> Lynn Goodman
> Fine Porcelain Pottery
> Cell 347-526-9805
> www.lynngoodmanporcelain.com

Lee Love on thu 28 aug 08


On Thu, Aug 28, 2008 at 8:42 PM, Lynn Goodman Porcelain Pottery
wrote:
> A day or so ago I asked for sources for strontium-bearing frits such
> as P-930, F-38 or Ferro 3292. No answer as of yet. Does anyone know
> where I can buy these frits?

Ferro Frit CC-257-2

http://ceramic-materials.com/cermat/material/492.html

Here is the Ferro webpage:

http://www.ferro.com/Our+Products/Tile+Coating+Systems/Products+galleries/Frits/


--
Lee Love in Minneapolis
http://mashikopots.blogspot.com/
http://claycraft.blogspot.com/

"Let the beauty we love be what we do.
There are hundreds of ways to kneel and kiss the ground." --Rumi

Peter on thu 28 aug 08


Lynn Goodman Porcelain Pottery wrote:
<as P-930, F-38 or Ferro 3292. No answer as of yet. Does anyone know
where I can buy these frits?>>

Ferro 3292 is listed in the Laguna catalog:
http://www.lagunaclay.com/catalog/pdf/lcc_frit.pdf

Best,
Peter
NM

Lynn Goodman Porcelain Pottery on thu 28 aug 08


A day or so ago I asked for sources for strontium-bearing frits such
as P-930, F-38 or Ferro 3292. No answer as of yet. Does anyone know
where I can buy these frits?

Thank you in advance!
Lynn


Lynn Goodman
Fine Porcelain Pottery
Cell 347-526-9805
www.lynngoodmanporcelain.com

Keith Arbogast on fri 29 aug 08


Lynn,
I bought F-38 directly from Fusion Ceramics. Its contact information
can be found at http://www.fusionceramics.com/ . A very kind lady
sent me a three pound sample at no charge when I first called to
inquire. When I called back to place an order, the lady said they
usually ship in thousands of pounds amounts, but she agreed to send
me a barrel of only 50 lbs.

Best wishes,
Keith Arbogast

Lynn Goodman Porcelain Pottery on fri 29 aug 08


Many thanks to all of you who posted the strontium frit info!

Lynn


Lynn Goodman
Fine Porcelain Pottery
Cell 347-526-9805
www.lynngoodmanporcelain.com