search  current discussion  categories  people 

public thank you to ron roy

updated wed 17 sep 08

 

Lois Sharpe on fri 12 sep 08


This is a public THANK YOU to Ron Roy for glaze help.

He has been most generous with time and information, and patience!

I greatly appreciate his help in fixing a funky glaze that I did not
want to give up on.

Thank you Ron.

lois




Lois Sharpe
Durham NC



Ron Roy on tue 16 sep 08


This was an interesting experiment - take out unwashed ash (about 15%) and
replace it with other materials.

I had a generic analysis for mixed washed wood ash - took out the ash and
replaced the oxides one for one using other materials - then designed a
short line blend using soda ash to replace the solubles in the unwashed
wood ash.

Another sample of just how powerful glaze calculation can be.

RR

>This is a public THANK YOU to Ron Roy for glaze help.
>
>He has been most generous with time and information, and patience!
>
>I greatly appreciate his help in fixing a funky glaze that I did not
>want to give up on.
>
>Thank you Ron.
>
>lois

Ron Roy
15084 Little Lake Road
Brighton, Ontario
Canada
K0K 1H0