search  current discussion  categories  wanted/for sale - for sale 

studio for sale/new hampshire

updated thu 11 sep 08

 

mel jacobson on wed 10 sep 08


Hello I have the following list for sale Located 10 Minutes from Portsmouth New Hampshire.
I will not ship. You must come and get. Sadly,I am forced to sell my
pottery equipment due to an injury that is preventing me from being able to
continue with pottery.I am selling the complete package only. It is all only
lightly used example- L&L 3 inch brick E23T kiln only fired 16 times. Price
is $15,000 List is long please remember to scroll to end. If interested my
email is "potteryinfo (at sign) gmail.com"-Mary Snow potteryinfo@yahoo.com

*EQUIPMENT*

L and L Kiln E23T 3 inch brick with furniture kit and vent sure

Paragon Caldera kiln test kiln and furniture kit plus extra shelf

VL Whisper Shimpo Wheel


Rolliing Thunder Slab roller


Bailey Model A400 Pugmill Steel De airing

i500w/ ac adaptor scale


23 boxes Clay tuckers smooth white/cs wh

Giffin Grip


respirator 54001 plus extra 2 filters


2 bucket sieves for glazing

Blender


measuring scops and spoons


pottery tools various


Jiffy Mixer 21 For mixing glazes 2-5 gallon

Lid master


Pot grippers


Shelving and tables

Rolltable with pugmill

Slabroller table

Glaze making Booth with vent

Partial Makings for SprayBooth

Spray gun-Never Used

*BOOKS*

The Potter's Encyclopedia of Color, Form and Decoration (Hardcover)2003

3rd Edition Electric Kiln Cermamics A guide to Clays and Glazes Zakin 2004


Ceramics Barrons 2002

Practical Solutions for Potters Gill Bliss 2001

The Glaze Book Stephen Murfitt 2002

HandMade Tiles frank Giorgini 2001

The Potters Primer Morgan Hall 2002

The Art of Handmade Tile 2002

Making Marks Discovering the Ceramixc Surface Robin Hopper 2004

The Potters Guide to Ceramic Surfaces Jo Connell Hard cover

The Clay Lover's guide to making molds Peirce Clayton

The Ceramic Glaze HandBook Mark Burleson

The Artists complete book of Health and SafetyGuide Monona Rossol

Mastering Cone 6 Glazes

The Ceramic Spectrum a simplified approach to Glaze & Color Development 2nd
edition

*Magazines*

Clay Times July August 2006 March April 2007 January February 2008

11 Pottery making Illustrated 2005-2008

Ceramics Monthly January 2007

*Chemicals*

Zircopax Plus 9.7ounces

Titanium dioxide 5lbs

Frit 3110 4 lbs 14.5 oz

Frit 3195 4 lbs

Frit 3124 70 lbs

Zinc oxide 4lbs 13 oz

Ravenscrag slip

Tin Oxide 2.5 lbs

Kiln Wash 11.9 oz

Boraq 11.6 oz

Nepheline syenite 98.5 lbs

magnesium carbonate 5 lbs

Granular Rutile 4lbs 12.6 oz

Silica 50lb

Epk 5lbs8oz

G200 feldspar 28lb 8 oz

Talc 38lbs

whiting 45 lbs

Wollastonite 28 lbs 8 oz

Yellow Ochre Iron 4lb 11.2 oz

Custer Feldspar 50 lb

copper carbonate 3lb 9.8oz

Black Iron Oxide 1lb 12.5
nickel oxde 8.5 oz

spanish iron oxide 4lb 7 oz 00

Dark rutile 1lb 7 oz

cobalt carbonate 15.8 oz

Bentonite 3lb 15.4 oz
chrome green Oxide 4lb

Dolomite 3 lbs

Borax 10.8 Oz

Soda Ash 1 lb 2.8 oz

Pyrotol (Alkatrol 2) 5lb 1.9 oz

Ball Clay 50 lbs

Om4 Ball Clay 3lbs 9oz

*GLAZING*

Mason Stains 6101 3.9 oz

6006 .8oz

6385 5oz

6324 4.8oz

6219 5.4 oz

5 GALLON Glaze Containers


Mastering cone 6 Glaze Licorice

Mastering cone 6 glaze Clear

Mastering Cone 6 majolica

Mastering cone 6 Robins Egg (teal blue)

Mastering cone 6 glaze Sky Blue

Floating blue

40 pint to quart size cone 6 glazes

9 mayco stroke and coat 2oz -
Grapel
Tigertail
Moddy Blue
Java bean
My blue heaven
Down to earth
Evergreen
Cottontail
Army Surplus

2 mayco stroke and coat 8 oz- Candy Apple and Hot Tamale

1 Mayco stroke and Coat 1 Pint- Cottontail

*And other miscellaneous items*


from minnetonka:
website http://www.visi.com/~melpots/
clayart site:
http://www.visi.com/~melpots/clayart.html