judy smith on fri 12 sep 08


I normally use cone 6 stoneware and bisque fire it to cone 04.=A0 I want to=
make some pots using low fire cone 06 stoneware clay.=A0 What cone setting=
=A0do I bisque fire the low fire clay to?=A0 =0A=0AThanks,=0AJudy Smith=0AN=