search  current discussion  categories  techniques - painting 

screening glaze/ great brush

updated tue 16 sep 08

 

Chuck T. Wagoner on mon 15 sep 08


I found a brush that is very good for forcing glaze through a fine mesh
screen.

The Libman 00523 Short Handle Tampico Scrub Brush.

It has a good handle at a good angle that is much easier to hold then a
straight handled paint brush.

I use a 90 mesh for the final screening of a glaze and it is hard to get the
Wallositinite through, this brush worked very well.

Available at places like Menards, it is really perfect for the job.

Chuck in Rockville, IN.