Alisa Clausen on tue 16 sep 08
Recipe Name: Randy's 3 in one Tim version
Cone: 6 Color:
Firing: Oxidation Surface: Glossy
Amount Ingredient
0
0
0
0 Total
Unity Oxide
0 Ratio
0 Exp
Comments: A glossy soft white glaze, a tiny bit fat. Evenly covering and
no effects of overlapping or breaking
| |
|