Hi,

I did this for a while, until I realised how much glaze I was wasting.

The compromise was a (dont laugh) very small plastic greenhouse =
(=A37.99) open on the front side, towels round the other 3 sides,banding =
wheel on ground. spray all pots with glaze a. change towels. spray all =
pots wirh glaze b. etc etc=20
Soak towels and reclaim glaze.
The other advantage of this is that if the wind changes direction, you =
dont get a sprayful back over your trousers!
Mask wearing all the time, of course.