search  current discussion  categories  glazes - misc 

glaze simulator download should work now..

updated fri 5 dec 97

 

Fraser /Suzette on thu 4 dec 97


My server told me that the self extracting files will not work through
Netscape. So I have changed the download files into (windows) zip files.
There are two hyperlinks on the page that will direct you to Winzip or
PkZip home pages where you can get free shareware if you are not so
equipped.
If you haven't lost all your patience yet give it another try...thanks.

fraserf@golden.net
www.golden.net/~fraserf

On another note I fired my fiber kiln today to a full cone 7. The firing
took 2 3/4 hours. This is longer than expected but the our weather was damp
and cold. Does anyone know if damp cold weather will extend firing time?