search  current discussion  categories  glazes - cone 4-7 

cone 6 salvation glaze?

updated thu 20 nov 08

 

Randy McCall on sun 16 nov 08


Has anyone used the Cone 6 Salvation Glaze to reglaze some pieces? Results?
Photos of results?


Randy

Cotton Patch Pottery
members.tripod.com/~McCallJ/index.html

iglasgo on wed 19 nov 08


Never tried that one. Recipe?

I use Strnad's Opal Blue as a salvation and it works over almost
anything. Looks great over high iron glazes. Melts from 04 to 6 and
doesn't run much.

Or I refire at 04 with a copper blue that makes a stunning forest
green over high iron glazes.

hth.