Roxanne Hunnicutt on mon 17 aug 09
0 whiting 25.0 50.0 125.0 silica 25.0 50.0 125.0 Kaolin 25.0 50.0 125.0 Fri=
t 3124 15.0 30.0 75.0 115.0 230.0 575.0 Boy oh boy do I have the glaze for =
you. This gives you the most LUSH
Leach Satin Clear from Leslie Lee R/OX x2 x5 custer 25.0 50.0 125.0 whiting
25.0 50.0 125.0 silica 25.0 50.0 125.0 Kaolin 25.0 50.0 125.0 Frit 3124 15.=
0
30.0 75.0 115.0 230.0 575.0 This gives you the most LUSH creamy satin
finish, you would not believe. AND IT IS CLEAR everywhere I have used it. I=
t
is so sweet. No craze, no pits, not problems.
Now can some GLAZE GURU tell me, should I test it with mason stains? And if
so should I use the ones marked to use with zinc, with out zinc or what.
WHERE IS THE ZINC?
IS there zinc within this glaze?
And can that same guru or his friends tell me, what colorants might work
best in this?
Rox
| |
|