My first tests of the Ohio fireclay body from the clay Tim Frederich
gave me. =3DA0 It is the unrefined fireclay 20 mesh with natural grog
added and just a dab of sagger clay,. =3DA0 With shino over it.

http://www.facebook.com/album.php?aid=3D3D108108&id=3D3D550727056&l=3D3D00f=
0ebe62=3D
1


--
Lee Love, Minneapolis
"The tea ceremony bowl is the ceramic equivalent of a sonnet: a
small-scale, seemingly constricted form that challenges the artist to
go beyond mere technical virtuosity and find an approach that both
satisfies and transcends the conventions." -- Rob Sliberman
full essay: http://togeika.multiply.com/journal/item/273/



--=3D20
--
Lee Love, Minneapolis
"The tea ceremony bowl is the ceramic equivalent of a sonnet: a
small-scale, seemingly constricted form that challenges the artist to
go beyond mere technical virtuosity and find an approach that both
satisfies and transcends the conventions." -- Rob Sliberman
full essay: http://togeika.multiply.com/journal/item/273/