search  current discussion  categories  tools & equipment - pug mills 

pugmills again

updated wed 16 sep 09

 

celia hirsh on tue 15 sep 09


Okay.
So we've heard from Melissa that the addition of epsom salts fails to
solve the problem of aluminum pitting and I can vouch the same for the
addition of vinegar.
So, I'm moving forward to another solution - an all stainless pug.
I see that Venco, an Australian company, makes a studio size (or at
least, my studio size) pugmill with a vacuum, called the Super Twin.
Does anyone have one? Do you like using it? Does it reclaim well?
Vacuum well?
Anyone in southern Ontario want to sell their used one?
Cheers,
Celia Hirsh
www.hirshpottery.com