Hello all and Arnold:
I have an error message today on my Paragon Kiln "FIL." which I do not see
on the manual. The firing was a cone 8 firing with firing down scheduled.
(ramp fired) The cycle seemed to be completed. (This would have been a $35
firing load usually, but I got a $31 for the firing cost reading) The cone =
7
not even half bent and the glaze appears to be slightly under-fired.
Thank you in advance for your input.
Thanks
May
--