search  current discussion  categories  glazes - crystalline 

slow cool crystal pix

updated sat 24 oct 09

 

mel jacobson on fri 23 oct 09


i have added the pix from bill merrill.
slow cool, several days
clayart page, click below.
he will add information in a post to clayart.
from: minnetonka, mn
website: http://www.visi.com/~melpots/
clayart link: http://www.visi.com/~melpots/clayart.html
new book: http://www.21stcenturykilns.com