For the interior of a vessel that has a copper red on the outside a
simple solution is to use the same base glaze (If it doesn't craze) and
leave out the copper. The Carlton Ball Chun glaze is a great copper
red. If you use an opacificer like zircopax in it you'll get a smooth
white , easy to clean interior etc. =3D20

=3D20

Bill Merrill