Hello all;

If my cone 8 on my kiln is end temp at 1238 C (2260 F) and hold at 8 min. I=
s
it safe to say if I minus 20 deg C (2224 F) and hold for 8 min , as a
starting point, to reach a cone 6 firing?

Thank you