search  current discussion  categories  glazes - misc 

vct glaze

updated tue 17 nov 09

 

Bill Merrill on mon 16 nov 09


For those of you interested in glazes names and where they come from, it =
=3D
is nice to give credit to the originator of a particular glaze if the =3D
author so to speak is known. The VCT glaze that was just mentioned in a =
=3D
post on recalculating a glaze from cone 10 to cone 6 was a glaze that =3D
was formulated by Val Cushing at Alfred many years ago. Just a personal =
=3D
note.....

Richard White on mon 16 nov 09


Bill, thanks for the additional info. I suspected as much from the VC in =
=3D
the
name, but had no means to confirm that from a source document. I'll note
that in the comments field of my personal database. It's a wonderful glaz=
=3D
e
at ^10; if we could only duplicate it at ^6...

dw