Alice Chittenden on tue 1 dec 09
Karen,
I concur with Snail - the borax is the culprit. I was told that the=3D20
Bringle slip could be mixed up without the borax. I was wondering if=3D20
anyone has tried this and how the resulting slip compares to the=3D20
original.
Alice Chittenden
| |
|