search  current discussion  categories  glazes - specific colors 

sos: mc6g - licorice & which brown glaze?

updated sun 13 dec 09

 

Shula on sat 12 dec 09


I can't find my MC6G. (I know it's around here somewhere) But I'd like to g=
laze some pots today and don't remember which brown glaze I put on the lip =
of a bowl on which I used licorice. I remember one of the browns was sugges=
ted to put over licorice, but I don't remember which one. Possibly waterfal=
l brown?

I'd really, really appreciate it if someone whose copy of MC6G is handy wou=
ld take a look and let me know.

Thanks

Shula
Desert Hot Springs, California USA

Shula
Desert Hot Springs, California USA
www.claymystique.etsy.com

John Hesselberth on sat 12 dec 09


Hi Shula,

Waterfall Brown was the one we showed in the book--but do that one and =3D
experiment with some others too. Lots of glazes look good in contrast =3D
with the glossy black of Licorice.

Regards,

John

On Dec 12, 2009, at 8:36 AM, Shula wrote:

> I can't find my MC6G. (I know it's around here somewhere) But I'd like =
=3D
to glaze some pots today and don't remember which brown glaze I put on =3D
the lip of a bowl on which I used licorice. I remember one of the browns =
=3D
was suggested to put over licorice, but I don't remember which one. =3D
Possibly waterfall brown?
>=3D20
>=3D20